I-aluminium titanate ceramic

Iimbonakalo

  • Ukunganyangeki okuqinisekileyo kwe-thermal
  • Max. Ubushushu obusebenzayo: I-900 ° C
  • Ulwandiso oluphantsi kakhulu (<1 × 10-6k-1 phakathi kwe-20 ne-600 ° C)
  • I-Tream yeTherithi ePhezulu (1.5 W / MK)
  • Imodyuli yoMncinci omncinci (17 ukuya kwi-20 GPA)
  • Ukungaxhathisi bekhemikhali
  • I-Holl Arhity ePhakamileyo ngeentsimbi ze-molten

Iinkcukacha zeMveliso

Iithegi zeMveliso

Izinto eziluncedo kwimveliso kunye neempawu

● Intsebenzo yokufakelwa kwe-irmal yokuphakama ichaphazela ngokuthe ngqo ireyithi yengcinezelo yoxinzelelo kunye nemigaqo yoxinzelelo ephantsi. Phakathi kwezixhobo ezikhoyo, i-Aluminium Timetatate Ceramics zilungile ngenxa yokuqhutywa komhlaba okuphantsi komhlaba, ukungavisisani okuphezulu kothusayo, kunye nokungavisisani kwe-aluminium ye-aluminium.

● Ukuhamba kwe-thermal ephantsi kunye nokungabeki kwe-Aluminium Tititate kungayinciphisa ngokufanelekileyo ukubetha kwinxalenye ephezulu yetyhubhu, qinisekisa ukugcwalisa uzinzo lwe-caving, kwaye uphucule umgangatho wokuphosa.

● Xa uthelekiswa ne-iron yentsimbi, i-carbon nitrogen, kunye ne-Silicon Nitride, i-Aluminium Tititata inonyango oluhle kakhulu, kwaye akukho nyango lungaphezulu kofakelo.

● Phakathi kwezinto ezininzi eziqhelekileyo ezisetyenziswayo ze-aluminium ezisetyenziswayo, i-Aluminium Timetate ineyona mpahla ingekho mgangathweni, kwaye akukho arhente yokuhlambela iyafuneka ukunqanda ungcoliseko kulwelo lwe-aluminium.

Amanyathelo okhuseleko ukuze asebenzise

.

● Ukongeza, ngenxa yamandla ayo aphantsi, ukhathalelo kufuneka lwenziwe ukunqanda amandla angaphandle echaphazela umbhobho xa ucoca umphezulu we-slag.

● I-Aluminium ye-Aluminite igcinwe kufuneka igcinwe yome ngaphambi kokufakwa, kwaye akufuneki isetyenziswe kwiindawo ezinamanzi okanye ezinamanzi.